Advanced packaging
Panel-Level Packaging Explained: Process, Applications, and Challenges
Quick answer
Panel-level packaging (PLP) is fan-out packaging carried out on a rectangular panel instead of a round 300 mm wafer. The dies are placed on a large carrier, molded into a reconstituted panel, and wired up with redistribution layers (RDLs) built directly on the molded surface [S4]. The two panel sizes written into SEMI standards are 510 × 515 mm and 600 × 600 mm [S3], although panels from 310 × 310 mm to 700 × 700 mm are in use or planned [S2]. The point of the larger, rectangular format is throughput and area: more packages per process step, and less unusable area at the edge than a circle leaves, an advantage that grows with package size [S2]. The price is that warpage, die shift, lithography and copper plating uniformity are all harder to control over a panel than over a wafer [S1][S2]. Fan-out panel-level packaging (FOPLP) is the panel version of fan-out wafer-level packaging (FOWLP), not a different package architecture.
Why it exists and how it works
Fan-out wafer-level packaging solved a specific problem: as components shrink, the established assembly flows no longer suit them, so the die is embedded in a molded body larger than itself and its contacts are redistributed outward over that body [S4]. Instead of a substrate, the die is embedded in mold compound, and the RDL fans the connections out over the molded area around it [S4]. In this page's reading, the reconstituted "wafer" is round because the equipment it inherited from front-end processing is round, not because the process needs a circle; a rectangular panel borrowed from the printed-circuit-board and display industries carries many more packages per batch [S1][S4].
The chips-first flow has four stages, in outline as Fraunhofer IZM described it in 2016: individual dies are placed face-down on a temporary carrier; the dies are over-molded into a reconstituted panel; the panel is released from the carrier; and the RDL is built on the exposed die faces and mold surface, either routing each die's pads outward or linking several dies together [S4][S1]. A chips-last variant builds the RDL first and places dies onto it afterwards, which protects known-good dies from RDL yield loss at the cost of tighter placement requirements [S2].
The geometry argument is simple and worth doing honestly. A 300 mm wafer with a 3 mm edge exclusion offers about 67,900 mm² of usable area; a 510 × 515 mm panel with a 10 mm edge exclusion offers about 242,600 mm², roughly 3.6 times as much. What matters to cost, though, is how many whole packages fit. On a square grid, centered on the wafer and aligned to the corner of the usable area on the panels, with no allowance for saw streets and no attempt to shift either grid for a better fit, 10 × 10 mm packages use 87% of the wafer's gross area (the whole 300 mm circle, exclusion included) and 91% of the panel's gross area; at 30 × 30 mm the wafer drops to 66% while the panel stays near 88%; a 310 × 310 mm panel, the smallest format in the reports, sits between the two at 76% [calculated for this page, assumptions as stated]. These are one layout's numbers, not the best attainable: shifting the grid can change them substantially, and saw streets lower all three. Industry sources describe a similar pattern: comparing a 300 mm wafer with a panel of about 300 mm, ASE says the panel's utilization advantage becomes significant above roughly 3.5 times the reticle size [S2]. The reticle field is the area a lithography scanner exposes in one shot, about 26 × 33 mm [S12].
Where it is used
Status matters more than names here, so the cases are grouped by status, and each item says whether it rests on the company's own statement or on a media report.
Volume production: Samsung Electro-Mechanics' own company history records a PLP business started in 2015 and transferred to Samsung Electronics in 2019, in the company's words to achieve synergy at the Samsung group level [S7]; that the business packaged the application processor of Samsung's Galaxy Watch in FO-PLP from 2018 on a single panel line is as reported by ET News in April 2019 [S7]. As reported by industry media: Nepes runs 600 × 600 mm panels (reported 2022 and 2025) [S1b][S2], and STMicroelectronics has replaced the leadframe of small QFN devices with fan-out RDLs (reported 2025) [S2].
Demonstrated or announced: ASE has shown a ten-chip, ten-bridge test vehicle on a 310 × 310 mm panel (demonstrated; as reported in 2025) [S2]; Amkor has stated that it is working toward 650 × 650 mm panels for production (announced; as reported in 2025) [S2]; Fraunhofer IZM's consortium work covers 610 × 457 mm panels and mold-first flows (demonstrated; the institute's own 2016 release and 2022 paper) [S1][S4]. A 2022 industry report listed further OSATs (outsourced assembly and test providers) and substrate makers as having either started FOPLP volume production or begun qualifying panel processes, without saying which company was at which stage [S1b].
Reported, with no status assigned here: a panel carrier at TSMC for very large interposers ("CoPoS"). TSMC said on its October 2026 earnings call that it is working on CoPoS [S11]; the panel sizes are from reports: a 310 × 310 mm format according to the equipment maker SCHMID (as reported in May 2026), with 510 × 515 and 600 × 600 mm described as the sizes being standardized across the wider ecosystem [S2][S10]. SpaceX is reported to be planning a 700 × 700 mm line (as reported in July 2025) [S2].
Alternatives and trade-offs
The alternative to a panel is the wafer the process came from, so the comparison is FOPLP against FOWLP. The table keeps to statements that have a source; where a line is qualitative, that is because the sources read for this page give no figure.
| FOWLP (300 mm wafer) | FOPLP (panel) | |
|---|---|---|
| Carrier | Round, 300 mm; the format that existing equipment, chucks and metrology were built for [S1] | Rectangular, 310 × 310 to 700 × 700 mm; SEMI-standard sizes 510 × 515 and 600 × 600 mm [S2][S3]; much tooling adapted from PCB and display lines [S1] |
| Area utilization | Lower for large packages because of the circular edge [S2] | Higher for large packages; ASE reports a significant gap above roughly 3.5× reticle size when comparing a 300 mm wafer with a panel of about 300 mm [S2] |
| Lithography | Steppers with reticle-size limits; well understood [S2] | Laser direct imaging is slower and needs off-line measurement; multi-head LDI shows stitching offsets; dry-film resists reached 3.5 µm lines and spaces, spray-coated liquid resist 2.5/1.5 µm in research [S1][S2] |
| Warpage | Present, from the gap in CTE (coefficient of thermal expansion) between silicon (~2.6 ppm/K) and mold compound (~7 ppm/K) [S2] | Significantly higher than on wafers for the same materials, by Amkor's account [S2]; dominated by carrier–EMC–die CTE mismatch plus EMC cure shrinkage [S1] |
| Die shift | Present; compensated with adaptive patterning [S5] | Larger with thinner over-mold and higher silicon density; adaptive patterning might be needed [S1] |
| Design data | Wafer-style design flows [interpretation] | PCB-style Gerber or ODB++ formats struggle at 2 µm lines and spaces [S1] |
| Yield exposure | Chips-first risks known-good dies on RDL yield; chips-last needs precise placement [S2] | The same, over a larger and more expensive batch per panel [interpretation] |
Engineering interpretation, and what is uncertain
The following is interpretation drawn only from the sources above.
Warpage on a panel is the wafer's warpage with longer lever arms. The CTE mismatch and cure shrinkage are the same materials problem, but displacement scales with the distance from the neutral point, and that distance is longer on a panel: the diagonal of a 510 × 515 mm panel is about 725 mm, against a 300 mm wafer diameter. That is why IZM's stated goal is warpage that stays controlled through every step rather than minimized at one step [S1]: a panel that is flat after molding but bows during RDL cure has still lost the lithography, and the later steps have less tolerance than the earlier ones.
Die shift is the reason adaptive patterning is considered for panels. Each die moves slightly as the mold compound flows and shrinks, on top of the placement tolerance of the die attach itself; a Deca and ASE design study simulates natural variation of about ±20 µm and ±0.1° at 3σ, values it describes as typical of production, and a Deca presentation shows Y-direction displacement after molding of −29 to +10 µm across one 600 mm panel before compensation [S5]. A fixed mask with oversized capture pads and undersized vias can absorb that on a wafer, but Deca reports that this conventional mitigation does not scale easily at bond-pad pitches around 40–45 µm [S5]; on a panel, the shift it has to absorb accumulates across hundreds of millimeters. Measuring every die's actual position and regenerating the RDL pattern for each panel is what IZM's fiducial-die approach and Deca's Adaptive Patterning both do [S1][S5]. It is the route toward finer routing on a panel that has already moved: IZM's paper describes development toward 2 µm lines and spaces [S1], and Deca's fine-line measurements were reported on wafers [S5]. The cost is an offline measurement step and a maskless lithography tool that is slower than a stepper [S2].
Copper plating uniformity on a panel is first a current-distribution problem. Across any large cathode the primary current distribution concentrates current at edges and corners, and on a thin seed layer the voltage drop from the contact to the center of the panel adds a terminal effect that starves the middle [S8]. On a larger panel the current has farther to travel through the seed layer, so the terminal effect is expected to grow with panel size. A vendor presentation on panel RDL plating lists variation in current-density distribution among the causes of poor plating performance, reports the plated height difference between lines and pads as a measured result, and discusses levelers, insoluble anodes, cell design and layout compensation as the levers [S6]. The interpretation is that a panel line cannot plate its way to uniformity by trimming the average current density alone; it has to shape the current field with cell design, anodes and layout, and the additive chemistry, levelers in particular, is one lever among those rather than a substitute for them.
What is uncertain, because the sources read for this page give no verifiable figure: the conditions under which the panel cost advantage holds once yield and equipment depreciation are included; production yield at lines and spaces below about 2 µm on full-size panels; and whether the reported large-interposer panel programs at the foundry level reach volume in the form described.
Further reading and sources
On this site: the Copper Electroplating Guide explains Faraday's law and why plating thickness is a current-density-times-time quantity; the Plating rate calibration guide shows how to fit measured thickness against time; the Engineering Unit Converter handles A/dm² and the other plating units; Chiplets Explained covers what is placed on these panels and why; Dual Damascene in Advanced Packaging covers the finest RDL, made by a different copper process from the panel RDL described here [S9].
Sources (grade A unless noted):
- T. Braun et al., "Panel Level Packaging – Where are the Technology Limits?", ECTC 2022 [S1]; reported in P. Garrou, IFTLE 532, 3D InCites, 2022 (B) [S1b].
- L. Peters, "The Rise of Panel-Level Packaging", Semiconductor Engineering, 24 July 2025 (B; individual company statements attributed in text) [S2].
- SEMI 3D20, Specification for Panel Characteristics for Panel Level Packaging Applications; SEMI E181, Panel FOUP; SEMI Standards Watch, December 2020 [S3].
- Fraunhofer IZM, "A milestone in manufacturing technology – fan-out panel level packaging", 7 July 2016 [S4].
- R. Davis, B. San Jose (Deca), J. Hunt, C.-P. Chen (ASE), "High-density Fan-Out Chip on Substrate using M-Series and Adaptive Patterning Technology", IMAPS Device Packaging Conference 2022; C. Sandstrom and T. Olson (Deca), "Mask-less Laser Direct Imaging & Adaptive Patterning for Fan-Out Heterogeneous Integration", IMAPS Device Packaging Conference presentation (slides dated March 7–10, 2022) (B; vendor figures) [S5].
- L. Kim et al., "Embedded Trace and RDL Copper Plating Process for Panel Level Packaging Applications", IMAPS DPC 2020 (B; vendor) [S6].
- Samsung Electro-Mechanics, company history (2010s), samsungsem.com: PLP business launched 2015, transferred to Samsung Electronics in 2019 (A); ET News, Samsung Electro-Mechanics FO-PLP for the Galaxy Watch AP, April 2019 (B) [S7].
- TrendForce News, "Equipment maker SCHMID flags TSMC panel-level packaging push, 310×310 mm progress", 19 May 2026, citing SCHMID's earnings call (B; equipment-vendor statement) [S10].
- TSMC, 3Q26 earnings conference call transcript, 15 October 2026 (A; company statement) [S11].
- ASML, TWINSCAN NXT:1965Ci product page, exposure field size (A) [S12].
- M. Schlesinger and M. Paunovic (eds.), Modern Electroplating, 5th ed., Wiley, 2010; J. W. Dini, Electrodeposition, Noyes, 1993 (current distribution chapters) [S8].
- On this site, by cross-reference: the Copper Electroplating Guide (Faraday's law and current-density units), the Plating rate calibration guide (least-squares thickness-versus-time fit), the Engineering Unit Converter, Chiplets Explained (citing S. Naffziger et al., ISCA 2021, and the TSMC CoWoS page) and Dual Damascene in Advanced Packaging (citing P. C. Andricacos et al., IBM J. Res. Dev. 1998) [S9].